Process Details
Equipment Plasmatherm 790
Technology RIE
Material Parylene
Mask Materials Photoresist
Gases Used O2


m_pary1 is an O2 etch that can be used for parylene and other polymers.

Parameters

Parameter Etch
RF Power 105 W
Pressure 100 mTorr
O2 Flow 99 sccm

Capabilities

Etch Rate

Mask Selectivity

Sidewall Profile

  • Undercut: XXX


Limitations

????

Qualification

Once a month m_pary1 is run on a XXX. This etch rate is reported in the chart below.