Line 82: Line 82:
 
[[File:SPR220 3um aligner grating silicon.jpg|1000px]]
 
[[File:SPR220 3um aligner grating silicon.jpg|1000px]]
  
===5µm of SPR 220 (3.0)===
+
==5µm of SPR 220 (3.0)==
 +
 
 +
==10µm - SPR 220 (3.0)==
 +
 
 +
===Process===
 +
# Dehydrate and apply HMDS
 +
# Spin
 +
# Bake ???
 +
# Wait ≥? min
 +
# Expose
 +
#* Stepper
 +
#** Silicon - ??
 +
#** Aluminum (~90% reflection) - ??
 +
#** ~15% reflection - ??
 +
#* Aligner - ? sec (silicon)
 +
# Wait ≥?? min
 +
# Bake 115°C for 90 sec
 +
# Develop
 +
#* ACS - AZ300 - ?? sec
 +
#* CEE - AZ726 ?? DP
  
 
==Technical Data Sheet==
 
==Technical Data Sheet==
 
* [https://drive.google.com/file/d/0B7eVu3mcqumAamhfcFFyRUxtRTA/view?usp=sharing| Data Sheet]
 
* [https://drive.google.com/file/d/0B7eVu3mcqumAamhfcFFyRUxtRTA/view?usp=sharing| Data Sheet]

Revision as of 09:01, 12 December 2018

SPR 220 is our most commonly used photoresist, especially for RIE. The lab stocks SPR 220 (3.0) for general use, in the ACS 200 Cluster Tool, and in the CEE 200X #1 & #2. For films thicker then 5µm SPR 220 (7.0) is also available from the LNF Store.


3µm - SPR 220 (3.0)

Process

  1. Dehydrate and apply HMDS
  2. Spin
  3. Bake 115°C for 90 sec
  4. Wait ≥5 min
  5. Expose
    • Stepper
      • Silicon - 0.40 sec
      • Aluminum (~90% reflection) - 0.34 sec
      • ~15% reflection - 0.42 sec
    • Aligner - 7 sec (silicon)
  6. Wait ≥3 min
  7. Bake 115°C for 90 sec
  8. Develop
    • ACS - AZ300 - 30 sec
    • CEE - AZ726 30-30 DP

Characterization

Stepper

Minimum Feature Size
Grating 700 nm
Line ??
Trench 1 µm
Hole ??
Pillar ?? nm

Gratings with equal duty cycle.

SPR220 3um stepper grating silicon.jpg SPR220 3um stepper grating aluminum.jpg SPR220 3um stepper grating low reflection.jpg

Free standing trenches.

SPR220 3um stepper trench 1um.jpg SPR220 3um stepper trench 700nm.jpg

Free standing lines.

  1. TODO

Holes

  1. TODO

Pillars

  1. TODO

Focus should be kept at 0.

SPR220 3um stepper focus.jpg

Puddle vs Spray Develop

  1. TODO

Spray develop time: SPR220 3um develop time.jpg

Contact Aligner

~2µm minimum feature size, but this is partially limited by the mask maker. SPR220 3um aligner grating silicon.jpg

5µm of SPR 220 (3.0)

10µm - SPR 220 (3.0)

Process

  1. Dehydrate and apply HMDS
  2. Spin
  3. Bake ???
  4. Wait ≥? min
  5. Expose
    • Stepper
      • Silicon - ??
      • Aluminum (~90% reflection) - ??
      • ~15% reflection - ??
    • Aligner - ? sec (silicon)
  6. Wait ≥?? min
  7. Bake 115°C for 90 sec
  8. Develop
    • ACS - AZ300 - ?? sec
    • CEE - AZ726 ?? DP

Technical Data Sheet