==Process List==
 
* [https://docs.google.com/document/d/1XiJQ3KrK1GPnzWqw2qyYfuVe62TWAFP0Sdi7DffMmJg/preview SU-8 Photolithography]
 
* [https://docs.google.com/document/d/1XiJQ3KrK1GPnzWqw2qyYfuVe62TWAFP0Sdi7DffMmJg/preview SU-8 Photolithography]
*: SU-8 is a negative, epoxy-based photoresist manufactured by MicroChem.  It is commonly used to make PDMS molds for microfluidics and other applications.  Several different series are available, and in each series, SU-8 is available in a range of viscosities.  The LNF provides several viscosities of the SU-8 2000 series. Product datasheets are available here:  [http://www.microchem.com/pdf/SU-82000DataSheet2000_5thru2015Ver4.pdf] [http://www.microchem.com/pdf/SU-82000DataSheet2100and2150Ver5.pdf]
+
*: SU-8 is a negative, epoxy-based photoresist manufactured by MicroChem.  It is commonly used to make PDMS molds for microfluidics and other applications.  Several different series are available, and in each series, SU-8 is available in a range of viscosities.  The LNF provides several viscosities of the SU-8 2000 series (SU-8 2005 & 2010 are included in cost of using Solvent Bench 94; SU-8 2050 & 2100 are recharged). Product datasheets are available here:  [http://www.microchem.com/pdf/SU-82000DataSheet2000_5thru2015Ver4.pdf] [http://www.microchem.com/pdf/SU-82000DataSheet2100and2150Ver5.pdf]
 
* [https://docs.google.com/document/d/1nLQS2AXEWX3MISWfj191QWd_zvJPhPvusSqXRn192KQ/preview PDMS Molding]
 
* [https://docs.google.com/document/d/1nLQS2AXEWX3MISWfj191QWd_zvJPhPvusSqXRn192KQ/preview PDMS Molding]
 
*: Polydimethylsiloxane (PDMS) is used to make microfluidics devices.  The LNF provides Sylgard 184 silicone elastomer made by Dow Corning.  This SOP describes the procedure for coating a mold with release agent, PDMS mixing and molding.  
 
*: Polydimethylsiloxane (PDMS) is used to make microfluidics devices.  The LNF provides Sylgard 184 silicone elastomer made by Dow Corning.  This SOP describes the procedure for coating a mold with release agent, PDMS mixing and molding.  

Latest revision as of 10:25, 11 September 2017

Warning Warning: This page has not been released yet.

This page lists the processes supported by the LNF for Solvent Bench 94.

Process List

  • SU-8 Photolithography
    SU-8 is a negative, epoxy-based photoresist manufactured by MicroChem. It is commonly used to make PDMS molds for microfluidics and other applications. Several different series are available, and in each series, SU-8 is available in a range of viscosities. The LNF provides several viscosities of the SU-8 2000 series (SU-8 2005 & 2010 are included in cost of using Solvent Bench 94; SU-8 2050 & 2100 are recharged). Product datasheets are available here: [1] [2]
  • PDMS Molding
    Polydimethylsiloxane (PDMS) is used to make microfluidics devices. The LNF provides Sylgard 184 silicone elastomer made by Dow Corning. This SOP describes the procedure for coating a mold with release agent, PDMS mixing and molding.
  • Temporary Bonding SOP
    This SOP explains temporary bonding of a sample to a carrier wafer with beeswax for lapping or polishing.