P5000 PECVD

230 bytes added, 4 years ago
|border=0
}}
 
=Information on film etch rates=
At this time, only BHF etch rates for two nitride films have been determined and reported by researchers
 
Etch rates for nitride in BHF:
200C Nitride = 535 A/min
400C Tensile Nitride = 215 A/min
 