Plasmatherm 790/Processes/L ox350

1 byte added, 1 year ago
|-
| Deposition Rate
| 744.2 Å5 nm/secmin
|-
| Index of Refraction
| 1.465467
|-
| Stress
| -380 420 MPa
|-
|}