*Parylene: 1.3 µm/min
*Platinum: ~1.5 nm/min
*SiO2SiO<sub>2</sub>: 28 nm/min*Aluminum: < 2 nm/min (varies with etch time; e.g. 30 sec or less is higher, ~4 nm/min)