Tempress S1T4 - LTO 6"
| Tempress S1T4 - LTO 6" | |
|---|---|
| Equipment Details | |
| Technology | LPCVD |
| Materials Restriction | Heavily-Restricted |
| Sample Size | 150mm |
| Gases Used | N2, O2, SiH4 |
| Equipment Manual | |
| Overview | System Overview |
| Operating Procedure | SOP |
| Supported Processes | LTO |
| Maintenance | Maintenance |
The Tempress diffusion system is a modular horizontal furnace designed to process silicon wafers as part of the manufacturing technology of semiconductor, optical, MEMS, and solar devices. LTO is formed by using a process called LPCVD, Low Pressure Chemical Vapor Deposition. Chemical vapor deposition forms thin films on the surface of a substrate by thermal decomposition and/or reaction of gaseous compounds. The desired material is deposited directly from the gas phase onto the surface of the wafer. The important factors are gas ratio, temperature, and pressure.
Contents
Announcements
- There are no announcements at this time.
Capabilities
- Low Temperature Oxide - LTO
- Maximum Thickness - 2µm
System overview
Hardware details
- N2 - Maximum flow 1 slpm
- N2 - Maximum flow 10 slpm
- O2 - Maximum flow 500 sccm
- SiH4 - Maximum flow 100 sccm
Substrate requirements
- Silicon only
- Can process up to 25, 150 mm (6") wafers
- Wafer thickness, ~675um for 150mm (6")
Material restrictions
Below is a list of approved materials for the tool. Approved means the material is allowed in the tool under normal circumstances. If a material is not listed, please create a helpdesk ticket or email info@lnf.umich.edu for any material requests or questions.
Supported processes
- Low Temperature Oxide - LTO
Process details
Characterization data
Standard operating procedure
Checkout procedure
- Create a Help desk Ticket requesting training.
- LNF staff will schedule a time for initial training. After completing training the user can attempt a checkout session. It may be necessary for some users to participate in more than one training session, prior to attempting check out.
- Schedule a checkout session with a tool engineer via the existing Helpdesk ticket. If this checkout is successful, the engineer will authorize you on the tool.
Maintenance
- Maintenance is performed on the tool, after 30-40µm of accumulated deposition.
- Maintenance consists of replacing the following quartz parts within the tube.
- Cage
- Twin rods
- Bridge for twin rods
- Injectors
- Dummy wafers
- Tube is replaced at 100µm of accumulated deposition.