Tempress S5T3 - Boron Diffusion 4"
The Tempress diffusion system is a modular horizontal furnace designed to process silicon wafers as part of the manufacturing technology of semiconductor, optical, MEMS, and solar devices. Diffusion refers to the process of intentionally introducing impurities into an extremely pure semiconductor in order to change its electrical properties. The diffusion process begins with the deposition of a high concentration of the desired impurity on the silicon surface. At high temperature the impurity atoms move, from the surface, further into the silicon crystal.
| Tempress S5T3 - Boron Diffusion 4" | |
|---|---|
| Equipment Details | |
| Technology | Thermal processing |
| Materials Restriction | CMOS Clean |
| Sample Size | 100mm |
| Gases Used | N2, O2 |
| Equipment Manual | |
| Overview | System Overview |
| Operating Procedure | SOP |
| Supported Processes | Boron Diffusion |
| Maintenance | Maintenance |
Contents
Announcements
- No announcements at this time.
Capabilities
System overview
Hardware details
- N2 - Maximum flow 10 slpm
- O2 - Maximum flow 10 slpm
- O2 - Maximum flow 500 sccm
- Techneglas Boron solid sources
Substrate requirements
- Silicon only
- Can process up to 16, 100 mm (4") wafers
- Wafer thickness, ~525um for 100mm (4")
Material restrictions
The Tempress S5T3 - Boron Diffusion 4" is designated as a CMOS Clean class tool. Below is a list of approved materials for the tool. Approved means the material is allowed in the tool under normal circumstances. If a material is not listed, please create a helpdesk ticket or email info@lnf.umich.edu for any material requests or questions.
Supported processes
Process details
- [https://docs.google.com/spreadsheets/d/1ZU80YAMVYkR08ptzQTmzpaY1KIWuR1H9eSsP9ctVqYk/preview#gid=312565195 Process recipe overview
Characterization data
Standard operating procedure
Checkout procedure
- Create a Help desk Ticket requesting training.
- A process engineer will schedule a time for initial training. After completing training the user can attempt a checkout session. It may be necessary for some users to participate in more than one training session, prior to attempting check out.
- Schedule a checkout session with a tool engineer via the Help desk Ticket system. If this checkout is successful, the engineer will authorize you on the tool.
Maintenance
- Replace Boron sources after ~200 hours of use.