Difference between revisions of "Xactix XeF2"

From LNF Wiki
Jump to navigation Jump to search
 
(4 intermediate revisions by the same user not shown)
Line 17: Line 17:
 
|maintenance = [https://docs.google.com/a/lnf.umich.edu/document/d/1PLT1HXSXWot4gJZBKRx-Dgn0VeV8OguIZgGq5gF8qIw/preview Maintenance]
 
|maintenance = [https://docs.google.com/a/lnf.umich.edu/document/d/1PLT1HXSXWot4gJZBKRx-Dgn0VeV8OguIZgGq5gF8qIw/preview Maintenance]
 
}}
 
}}
 +
 
The Xactix Xetch X.3.B is a [[Xenon difluoride|xenon difluoride]] etching tool that will etch [[Silicon|silicon]], [[Molybdenum|molybdenum]], and [[Germanium|germanium]] isotropically.  XeF<sub>2</sub> is a solid at atmosphere but will sublimate at vacuum.  The tool uses two expansion chambers to alternatively sublimate the XeF<sub>2</sub> and release it into the etch chamber. The etch rate is highly dependent on the chamber's loading.  A wafer with only a thin trench exposed will etch very fast where as a blanket 100 mm Si wafer may etch as slow as 800 Å/cycle.  Wafers are manually loaded directly into the chamber, and the tool can accommodate pieces up to 150 mm wafers.
 
The Xactix Xetch X.3.B is a [[Xenon difluoride|xenon difluoride]] etching tool that will etch [[Silicon|silicon]], [[Molybdenum|molybdenum]], and [[Germanium|germanium]] isotropically.  XeF<sub>2</sub> is a solid at atmosphere but will sublimate at vacuum.  The tool uses two expansion chambers to alternatively sublimate the XeF<sub>2</sub> and release it into the etch chamber. The etch rate is highly dependent on the chamber's loading.  A wafer with only a thin trench exposed will etch very fast where as a blanket 100 mm Si wafer may etch as slow as 800 Å/cycle.  Wafers are manually loaded directly into the chamber, and the tool can accommodate pieces up to 150 mm wafers.
  
 
{{Caution|This system is not for deep silicon etching.}}
 
{{Caution|This system is not for deep silicon etching.}}
 +
 +
  
 
==Capabilities==
 
==Capabilities==
Line 34: Line 37:
 
*Doesn’t quickly attack [[Deep reactive ion etching|BOSCH process passivation layer]]
 
*Doesn’t quickly attack [[Deep reactive ion etching|BOSCH process passivation layer]]
 
* [http://www.xactix.com/XeF2_Unique.pdf Additional Info]
 
* [http://www.xactix.com/XeF2_Unique.pdf Additional Info]
 +
 +
  
 
==System Overview==
 
==System Overview==
Line 83: Line 88:
 
==Checkout Procedure==
 
==Checkout Procedure==
 
<!-- Describe the checkout procedure for the tool. For example: -->
 
<!-- Describe the checkout procedure for the tool. For example: -->
# Read through this page and the Standard Operating Procedure above.
+
# Read through the User Manual above.
 
# Complete the SOP quiz [https://docs.google.com/a/lnf.umich.edu/forms/d/1joXIQksqSQo-I_TNss3e_YG7LFMTAOjzebgSZfzJGck/viewform here].
 
# Complete the SOP quiz [https://docs.google.com/a/lnf.umich.edu/forms/d/1joXIQksqSQo-I_TNss3e_YG7LFMTAOjzebgSZfzJGck/viewform here].
# Create a [http://ssel-sched.eecs.umich.edu/sselScheduler/ResourceContact.aspx?tabindex=3&path=0:0:0:15000 helpdesk] ticket requesting training.
+
# Complete the [https://docs.google.com/forms/d/e/1FAIpQLSf4FcYP1XIoE-scXpXtmaegIzceSVe3uaR8e9P3K3LQAvn20w/viewform process request form].
# A tool engineer will schedule a time for initial training.
+
# Create a [http://ssel-sched.eecs.umich.edu/sselScheduler/ResourceContact.aspx?tabindex=3&path=0:0:0:{{#var:toolid}} helpdesk ticket] requesting a checkout session.
# Schedule a checkout session with a tool engineer via the helpdesk ticket system. If this checkout is successful, the engineer will authorize you on the tool.
+
# Authorization will be provided pending successful completion of the quiz and demonstration of proper tool use in the presence of a tool engineer.
 
 
For a successful checkout session, the user must demonstrate operation of the tool in adherence with this SOP without assistance from the tool owner.  We encourage users to use the SOP during the checkout as a guide.
 
  
 
==Maintenance==  
 
==Maintenance==  

Latest revision as of 07:59, 13 October 2021



Xactix XeF2
15000.jpg
XeF2 etching tool
Equipment Details
Technology Etching
Materials Restriction Semi-Clean
Material Processed Si, Mo and Ge
Mask Materials Pr
Sample Size Pieces to 150 mm
Gases Used XeF2
Equipment Manual
Overview Overview
Operating Procedure SOP
Supported Processes Supported Processes
Maintenance Maintenance


The Xactix Xetch X.3.B is a xenon difluoride etching tool that will etch silicon, molybdenum, and germanium isotropically. XeF2 is a solid at atmosphere but will sublimate at vacuum. The tool uses two expansion chambers to alternatively sublimate the XeF2 and release it into the etch chamber. The etch rate is highly dependent on the chamber's loading. A wafer with only a thin trench exposed will etch very fast where as a blanket 100 mm Si wafer may etch as slow as 800 Å/cycle. Wafers are manually loaded directly into the chamber, and the tool can accommodate pieces up to 150 mm wafers.


Capabilities


System Overview

Hardware Details

  • Gases
    • XeF2
    • N2
  • Pressure
    • 0 - 6 Torr XeF2
    • 0 - 20 Torr N2

Substrate Requirements

  • Pieces to 150 mm
  • No mounting required

Material Restrictions

The Xactix XeF2 is designated as a Semi-Clean class tool. Below is a list of approved materials for the tool. Approved means the material is allowed in the tool under normal circumstances. If a material is not listed, please create a helpdesk ticket or email info@lnf.umich.edu for any material requests or questions.


Supported Processes

A table of etch rates for the standard process can be seen below, these were all run with 20 second cycle times and 3 Torr XeF2 pressure. More process information for this tool can be found on it's supported processes

Material Size % Open Area Etch Rate (Å/cycle)
Si 100 mm 100% 800
Si 1 cm2 100% 10,000
SPR 220 100 mm 100% < 5

Standard Operating Procedure

Widget text will go here.

Checkout Procedure

  1. Read through the User Manual above.
  2. Complete the SOP quiz here.
  3. Complete the process request form.
  4. Create a helpdesk ticket requesting a checkout session.
  5. Authorization will be provided pending successful completion of the quiz and demonstration of proper tool use in the presence of a tool engineer.

Maintenance

Every other week the chambers leak rate is checked along with the XeF2 usage.